mig and flux core tips and techniques, equipment, filler metal
welder in training
- welder in training
-
New Member
-
Posts:
-
Joined:Fri Mar 16, 2012 2:20 pm
So I'm in school for combination welding. Right now I'm working on 4g open root. I have no problem penitrating to get flush on the back side of the workpiece but my instructor insists that I have atleast 1/16" build up on the back. I have no idea how to achieve this. I've been running slower, colder, hotter, faster. Is it all in the work angle? Please help. Voltage is at 16.3, wfs is at 150 and I'm running a big 1/32" open root gap. By the way, my 1, 2, and 3g all penetrated to flush but no build up also.
- weldin mike 27
-
Weldmonger
-
Posts:
-
Joined:Fri Apr 01, 2011 10:59 pm
-
Location:Australia; Victoria
Hi there,
I think as long as your penno is fully fused and not "sucked back" you are going well. 1/16 seems like a lot of build up in an over head weld. Jody recently made a video on this weld. on this site. Oh, if an instructor gives you a task that seems hard, hand them the shield and ask them to show you. If you're gunna talk the talk, you have to be able to walk the walk.
Mick
I think as long as your penno is fully fused and not "sucked back" you are going well. 1/16 seems like a lot of build up in an over head weld. Jody recently made a video on this weld. on this site. Oh, if an instructor gives you a task that seems hard, hand them the shield and ask them to show you. If you're gunna talk the talk, you have to be able to walk the walk.
Mick
welder in training
- welder in training
-
New Member
-
Posts:
-
Joined:Fri Mar 16, 2012 2:20 pm
Thanx for the input. After carefull examination of the weld, I did notice a bit of suck-back but just a hair. Any tips for just a bit more penotration? By the way, I did ask him to show me how to do it and he did get about 1/32". The problem is, his tip of staying to one side of the gap and letting it blow back into the gap isn't helping me much. Maybe its just lack of experience on my part. I don't know.
- weldin mike 27
-
Weldmonger
-
Posts:
-
Joined:Fri Apr 01, 2011 10:59 pm
-
Location:Australia; Victoria
Hi there,
Sorry. Ive got no tips as i dont do this type of weldinOn tghe experience side you you do things long enough, you do little things without even thinking about and they can be hard to explain. Maybe try dragging the gun so that the metal is being forced backwards. Only a slight angle of about 30°.
might help.
Mick
Sorry. Ive got no tips as i dont do this type of weldinOn tghe experience side you you do things long enough, you do little things without even thinking about and they can be hard to explain. Maybe try dragging the gun so that the metal is being forced backwards. Only a slight angle of about 30°.
might help.
Mick
welder in training
- welder in training
-
New Member
-
Posts:
-
Joined:Fri Mar 16, 2012 2:20 pm
Thanx for the tip. I actually gave that a try last night with a circular pattern and it seemed to work. Part of my problem was I was running a tight weave pattern. Thanx again. I'm sure I will be back on here with some more questions soon...going to 6g pipe.
- weldin mike 27
-
Weldmonger
-
Posts:
-
Joined:Fri Apr 01, 2011 10:59 pm
-
Location:Australia; Victoria
- weldin mike 27
-
Weldmonger
-
Posts:
-
Joined:Fri Apr 01, 2011 10:59 pm
-
Location:Australia; Victoria
Hey there,
Not sure if you have seen this video, Jody made it about a month ago or so. He explains it pretty well.
http://www.youtube.com/watch?v=uWv26K8r ... AAAAAAAAAA
Look at his root pass. Thats about as good as it gets. If Jody cant get 1/16 penno, then no one can.
Mick
Not sure if you have seen this video, Jody made it about a month ago or so. He explains it pretty well.
http://www.youtube.com/watch?v=uWv26K8r ... AAAAAAAAAA
Look at his root pass. Thats about as good as it gets. If Jody cant get 1/16 penno, then no one can.
Mick
Return to “Mig and Flux Core - gas metal arc welding & flux cored arc welding”
Jump to
- Introductions & How to Use the Forum
- ↳ Welcome!
- ↳ Member Introductions
- ↳ How to Use the Forum
- ↳ Moderator Applications
- Welding Discussion
- ↳ Metal Cutting
- ↳ Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding
- ↳ Mig and Flux Core - gas metal arc welding & flux cored arc welding
- ↳ Stick Welding/Arc Welding - Shielded Metal Arc Welding
- ↳ Welding Forum General Shop Talk
- ↳ Welding Certification - Stick/Arc Welding, Tig Welding, Mig Welding Certification tests - Welding Tests of all kinds
- ↳ Welding Projects - Welding project Ideas - Welding project plans
- ↳ Product Reviews
- ↳ Fuel Gas Heating
- Welding Tips & Tricks
- ↳ Video Discussion
- ↳ Wish List
- Announcements & Feedback
- ↳ Forum News
- ↳ Suggestions, Feedback and Support
- Welding Marketplace
- ↳ Welding Jobs - Industrial Welding Jobs - Pipe Welding Jobs - Tig Welding Jobs
- ↳ Classifieds - Buy, Sell, Trade Used Welding Equipment
- Welding Resources
- ↳ Tradeshows, Seminars and Events
- ↳ The Welding Library
- ↳ Education Opportunities