Can pure Argon used to migging stainless steel?? This is because in my living place we cant find trimix. Or what gas is used to replace trimix??? They only have Argon, CO2 and He here. No mix gas.

Any suggestions?? Thank you.

Steph.
Miller Syncrowave 250 DX
Hypertherm Powermax65
User avatar
  • Posts:
  • Joined:
    Fri Feb 12, 2010 10:48 am
  • Location:
    YOUNGSTOWN, OHIO

FCAW - 100% CO2 or Argon/CO2 The voltage may be somewhat lower if argon with 20 to 25 percent CO2 mixtures is selected. Generally, a gas flow rate of 40 cfh is suggested. Adjustments can be made, depending upon the specifics of the application.

GMAW - Spray Transfer - Use Argon and 1% to 2% - Oxygen. 99% argon - 1% oxygen is predominantly used , 98% argon, 2% oxygen when welding thinner material.
Short Circuiting Transfer - 90% helium, 7.5% argon, 2.5% CO2
Jim
Pipefitter/Weldor out of Local 396
Millermatic 252
Dynasty 200DX
Maxstar 150 STL
Spoolmate 100
Hypertherm Powermax 85
Miller Digital Elite
JD2 Model 32 Bender
Emerson 7120 Horizontal/Vertical Bandsaw
Oxy-Gas Torch outfit
Generac XP8000E Generator
User avatar
  • Posts:
  • Joined:
    Fri Apr 01, 2011 10:59 pm
  • Location:
    Australia; Victoria

Hi there,

Here is a link to an Australian gas supplier. How ever it answers the question that you asked.

http://www.bocworldofwelding.com.au/shi ... teels.html

Mick