mig and flux core tips and techniques, equipment, filler metal
Post Reply
bigworm40
  • Posts:
  • Joined:
    Sat Dec 06, 2014 4:58 pm

Can someone please tell me what the white substance along the edges of the weld is.
Attachments
20160225_125659.jpg
20160225_125659.jpg (40.84 KiB) Viewed 1166 times
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

8-)
Last edited by jeffBrian on Tue Mar 15, 2016 1:06 am, edited 1 time in total.
bigworm40
  • Posts:
  • Joined:
    Sat Dec 06, 2014 4:58 pm

A570 GR 50
75/25
Lincoln 71A85 Ultracore FCAW G
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

Probably just contaminates from the steel being dirty. can you explain what where or when this is happening. a lot of times people over think the problem and it's something really simple to fix. this may be the case here.
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

are you running correct gas for the wire?
Screenshot_2016-02-25-14-12-19.png
Screenshot_2016-02-25-14-12-19.png (323.13 KiB) Viewed 1134 times
bigworm40
  • Posts:
  • Joined:
    Sat Dec 06, 2014 4:58 pm

Yes 75/25
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

everything I've seen so far says high argon concentrations work best. the cfh rate is 40 to 50 also which is a higher flow. perhaps trying a higher concentrate of argon gas and check flowrate. other than that I'm still looking a bit. it's interesting because I've worked with guys who worked shipyards in Seward and I bet this wire is used. I wish someone else would stab at this with me.
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

could you try 85/15? here is just an explanation of the argon mixtures
Screenshot_2016-02-25-14-51-05.png
Screenshot_2016-02-25-14-51-05.png (498.79 KiB) Viewed 1121 times
Poland308
  • Posts:
  • Joined:
    Thu Sep 10, 2015 8:45 pm
  • Location:
    Iowa

Where did the metal come from? Is it steel or some grade of SS ? Is it galvanized or from a corrosive enviroment? I've seen some weird stuff bubble up through or from contaminated metals.
I have more questions than answers

Josh
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

bigworm40 wrote: A570 GR 50
75/25
Lincoln 71A85 Ultracore FCAW G
here's his response from earlier
Poland308
  • Posts:
  • Joined:
    Thu Sep 10, 2015 8:45 pm
  • Location:
    Iowa

I was wondering if it was used and maybe permiated with some kind of chemical.
I have more questions than answers

Josh
jeffBrian
  • Posts:
  • Joined:
    Sun Jan 31, 2016 1:36 am
  • Location:
    not the right place

I would get two maybe 3 other pieces of test material and run a bead on each. that should give you a better idea what's going on.
I don't think you specified if it was giving you this with just the one material you posted a pic of or all pieces. if you're wanting to know what's bubbling out of the metal just out of curiosity then I totally missed that. ... and now I feel dumb haha