Page 1 of 1

TIG + MS

Posted: Tue Jan 26, 2010 5:08 pm
by gnabgib
Did some welds yesterday on ms and overall I've been producing my best work using TIG but some of the beads developed a very slight wrinkled effect along them. I was joining 2 different thickness pieces, 5mm and 2mm so I suspect this was the cause...?

Re: TIG + MS

Posted: Tue Jan 26, 2010 7:43 pm
by rickbreezy
its not the thickness of the metal, ussually a wrinkled look to the weld is a sign of lack of gas protection in tig, or any gas protected welding process. turn the gas up, or get a bigger gas cup.

-rick

Re: TIG + MS

Posted: Tue Jan 26, 2010 11:38 pm
by gnabgib
rickbreezy wrote:its not the thickness of the metal, ussually a wrinkled look to the weld is a sign of lack of gas protection in tig, or any gas protected welding process. turn the gas up, or get a bigger gas cup.

-rick
Hmm..Not sure about that, as I was doing identical welds before and after using the same gas flow with exactly the same machine settings and less than half the runs were effected.