Tig welding tips, questions, equipment, applications, instructions, techniques, tig welding machines, troubleshooting tig welding process
Machine is Dynisty 350 base metal nickel alloy .093 -.093 t joint filler rod 718 ni in a fixture with long electrode stick out I have ran the joint 4 times same results pin hole in the root need help anything would help
dirtmidget33
- dirtmidget33
-
Heavy Hitter
-
Posts:
-
Joined:Tue May 13, 2014 5:22 pm
Bead looks very wide with another pass over it. Second pass looks like a wash to attempt to smooth out weld. as wide as the bead looks would say arc length is way too long spreading out arc so your not able to focus arc in root. This also causes voltage to increase and puts excessive heat into part. Keep a very tight arc length and focus arc in root. One pass on .093 should be more then sufficient. Plus maintain good torch angle. Looks like excessive filler causing distortion along with excessive heat causing distortion too.
Grabbed this off web for you
Pic is from lincoln web
http://www.lincolnelectric.com/en-us/su ... gle.com%2F
Pic taken from http://www.twi-global.com/technical-kno ... ities-066/
Grabbed this off web for you
- weld-fusion5.jpg (15.6 KiB) Viewed 462 times
http://www.lincolnelectric.com/en-us/su ... gle.com%2F
- jk66f4.gif (16.58 KiB) Viewed 465 times
why use standard nozzles after gas lens where invented. Kinda of like starting fires by rubbing sticks together.
- LtBadd
-
Weldmonger
-
Posts:
-
Joined:Sun Apr 12, 2015 4:00 pm
-
Location:Clearwater FL
-
Contact:
Good advice, make sure base material and filler are clean, keep the filler in the argon shield between dips.dirtmidget33 wrote:Bead looks very wide with another pass over it. Second pass looks like a wash to attempt to smooth out weld. as wide as the bead looks would say arc length is way too long spreading out arc so your not able to focus arc in root. This also causes voltage to increase and puts excessive heat into part. Keep a very tight arc length and focus arc in root. One pass on .093 should be more then sufficient. Plus maintain good torch angle. Looks like excessive filler causing distortion along with excessive heat causing distortion too.
Richard
Website
Website
Return to “Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding”
Jump to
- Introductions & How to Use the Forum
- ↳ Welcome!
- ↳ Member Introductions
- ↳ How to Use the Forum
- ↳ Moderator Applications
- Welding Discussion
- ↳ Metal Cutting
- ↳ Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding
- ↳ Mig and Flux Core - gas metal arc welding & flux cored arc welding
- ↳ Stick Welding/Arc Welding - Shielded Metal Arc Welding
- ↳ Welding Forum General Shop Talk
- ↳ Welding Certification - Stick/Arc Welding, Tig Welding, Mig Welding Certification tests - Welding Tests of all kinds
- ↳ Welding Projects - Welding project Ideas - Welding project plans
- ↳ Product Reviews
- ↳ Fuel Gas Heating
- Welding Tips & Tricks
- ↳ Video Discussion
- ↳ Wish List
- Announcements & Feedback
- ↳ Forum News
- ↳ Suggestions, Feedback and Support
- Welding Marketplace
- ↳ Welding Jobs - Industrial Welding Jobs - Pipe Welding Jobs - Tig Welding Jobs
- ↳ Classifieds - Buy, Sell, Trade Used Welding Equipment
- Welding Resources
- ↳ Tradeshows, Seminars and Events
- ↳ The Welding Library
- ↳ Education Opportunities