Tig welding tips, questions, equipment, applications, instructions, techniques, tig welding machines, troubleshooting tig welding process
Post Reply
Dirtynails
  • Posts:
  • Joined:
    Sun Oct 26, 2014 1:49 pm

Anyone use 1% Thoriated (yellow) 3/32 tungstens? How does the 1% compare to the 2%?
User avatar

Dirtynails wrote:Anyone use 1% Thoriated (yellow) 3/32 tungstens? How does the 1% compare to the 2%?
Does your supplier offer the 1%? Personally I've never seen the 1%
Richard
Website
Dirtynails
  • Posts:
  • Joined:
    Sun Oct 26, 2014 1:49 pm

It's some old stock made by Osram/Sylvania.
88MOOSE88
  • Posts:
  • Joined:
    Fri Jul 11, 2014 11:13 am
  • Location:
    Grimsby, united kingdom

2% carries the heat better, I've founded with 2% if you accidentally dip the tip goes all furry and the heat isn't directed as much.

with aluminium is not much use, the ball dances around and doesn't seem to stabilize.
Dirtynails
  • Posts:
  • Joined:
    Sun Oct 26, 2014 1:49 pm

Screen shot 2015-09-19 at 3.52.25 PM.png
Screen shot 2015-09-19 at 3.52.25 PM.png (216.12 KiB) Viewed 777 times
Dirtynails
  • Posts:
  • Joined:
    Sun Oct 26, 2014 1:49 pm

Any thoughts as to how much current a 3/32 yellow will handle regularly?
Dirtynails
  • Posts:
  • Joined:
    Sun Oct 26, 2014 1:49 pm

Screen shot 2015-09-19 at 4.24.58 PM.png
Screen shot 2015-09-19 at 4.24.58 PM.png (53.61 KiB) Viewed 769 times
CanMoulder
  • Posts:
  • Joined:
    Wed Apr 22, 2015 1:02 pm
  • Location:
    Ontario Canada

For the welding i do at work i use mostly 1% (yellow) and don't really find a difference between 1% and 2%
work just got the E3 ( purple) and the guys seems to like it
I need to finish out the 10-15 i have on the go befor i try something else

Sorry no help here

Kev