Ive been building MOTORSPORTS roll cages for about 3 years now. When I first started building them at a race shop I used to work at, my boss had me MIG weld the joints. Now that I have my own fab business, I have been TIG welding all the joints. Looks better and I like not having all the spatter over the cage.
Most of the cages I build are DOM 1.5" .120 wall. I've been using a 3/32" electrode with 1/16" filler. I was just watching one of Jody's video's again and he used 1/16" rod to tack the joints and then 1/8 rod for the welding. Was wondering if there is any benefit to using the bigger rod for the joint welds other than not having to dip as often and/or dipping it as much. I guess I've just used the 1/16" rod just because I can keep a tighter arc and have a tighter bead.
Is this just a kind of "personal preference" kind of thing, or would I get better penetration with adding more material with the larger rod?
-Caleb
Tig welding tips, questions, equipment, applications, instructions, techniques, tig welding machines, troubleshooting tig welding process
- Otto Nobedder
-
Weldmonger
-
Posts:
-
Joined:Thu Jan 06, 2011 11:40 pm
-
Location:Near New Orleans
The only distinction that comes to mind for me is a smaller heat-affected zone with the larger rod. The justification being, as soon as the puddle is hot enough to accept the 1/8" rod, that dip cools the puddle more than a similar dip from a 1/16" rod.
I think this is going to fall in the "personal preference" category until someone can show me some empirical evidence. Comparing the size of HAZ's for the different filler sizes would be a valid example.
I doubt you'll see a difference in penetration, if you're handling the rod effectively.
Steve S
I think this is going to fall in the "personal preference" category until someone can show me some empirical evidence. Comparing the size of HAZ's for the different filler sizes would be a valid example.
I doubt you'll see a difference in penetration, if you're handling the rod effectively.
Steve S
- big gear head
-
Ace
-
Posts:
-
Joined:Thu May 07, 2015 11:46 am
-
Location:KY.
I use 1/16 filler too. It's easier for me to run a smaller bead with the smaller rod. I hadn't considered the HAZ.
Freddie
Jet City Fab
- Jet City Fab
-
New Member
-
Posts:
-
Joined:Fri Jul 24, 2015 6:12 pm
That is a good point. I'll have to do a test on scrap pieces and see what the differences are. Thanks for the input Steve.
Return to “Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding”
Jump to
- Introductions & How to Use the Forum
- ↳ Welcome!
- ↳ Member Introductions
- ↳ How to Use the Forum
- ↳ Moderator Applications
- Welding Discussion
- ↳ Metal Cutting
- ↳ Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding
- ↳ Mig and Flux Core - gas metal arc welding & flux cored arc welding
- ↳ Stick Welding/Arc Welding - Shielded Metal Arc Welding
- ↳ Welding Forum General Shop Talk
- ↳ Welding Certification - Stick/Arc Welding, Tig Welding, Mig Welding Certification tests - Welding Tests of all kinds
- ↳ Welding Projects - Welding project Ideas - Welding project plans
- ↳ Product Reviews
- ↳ Fuel Gas Heating
- Welding Tips & Tricks
- ↳ Video Discussion
- ↳ Wish List
- Announcements & Feedback
- ↳ Forum News
- ↳ Suggestions, Feedback and Support
- Welding Marketplace
- ↳ Welding Jobs - Industrial Welding Jobs - Pipe Welding Jobs - Tig Welding Jobs
- ↳ Classifieds - Buy, Sell, Trade Used Welding Equipment
- Welding Resources
- ↳ Tradeshows, Seminars and Events
- ↳ The Welding Library
- ↳ Education Opportunities