New to Tig Welding, I am a hobbiest and I've used and "mastered" other processes. I got some pictures here and was wondering if I can get some little tips.
Attachments
IMG_3414.JPG
IMG_3414.JPG (37.7 KiB) Viewed 1520 times
IMG_3412.JPG
IMG_3412.JPG (34.75 KiB) Viewed 1520 times
IMG_3411.JPG
IMG_3411.JPG (38.2 KiB) Viewed 1520 times
User avatar

Welcome Juliano
The dark tungsten, you need more post flow time

Tell us what machine you have, and your settings
Richard
Website
tweake
  • Posts:
  • Joined:
    Mon Dec 18, 2017 4:53 am
  • Location:
    New Zealand

add to the above,

what are you welding?
is it cleaned?
what gas are you running?
thats some funking looking marking around the welds.
tweak it until it breaks
Juliano_R
  • Posts:
  • Joined:
    Wed Aug 14, 2019 9:28 pm

I got an eastwood tig 200, I have a 75% co2 argon mix @ 15 cfh and running with a 3/32 tungsten set at 110 amps. The steel is 3/16" and it wasn't cleaned before use. I know that it should be cleaned with a wire brush but I was too lazy to pull out the grinder :roll: . However I don't dip the tungsten in the weld pool and it still has trouble keeping a pointy tip.
Juliano_R
  • Posts:
  • Joined:
    Wed Aug 14, 2019 9:28 pm

Juliano_R wrote:I got an eastwood tig 200, I have a 75% co2 argon mix @ 15 cfh and running with a 3/32 tungsten set at 110 amps. The steel is 3/16" and it wasn't cleaned before use. I know that it should be cleaned with a wire brush but I was too lazy to pull out the grinder :roll: . However I don't dip the tungsten in the weld pool and it still has trouble keeping a pointy tip.
forgot to mention, running 0.1s pre flow and 4seconds post flow
tweake
  • Posts:
  • Joined:
    Mon Dec 18, 2017 4:53 am
  • Location:
    New Zealand

Juliano_R wrote:, I have a 75% co2 argon mix
thats why its all funky and probably why the electrode is looking bad.
you need 100% argon.
tweak it until it breaks
Juliano_R
  • Posts:
  • Joined:
    Wed Aug 14, 2019 9:28 pm

I though you needed 100% argon just for aluminium
tweake
  • Posts:
  • Joined:
    Mon Dec 18, 2017 4:53 am
  • Location:
    New Zealand

Juliano_R wrote:I though you needed 100% argon just for aluminium
with tig you need argon for everything.
with mig you need argon for aluminium.
thats one reason i prefer tig. you can use one gas with everything.
with mig you need to change the gas for each material and even material size.
tweak it until it breaks
Juliano_R
  • Posts:
  • Joined:
    Wed Aug 14, 2019 9:28 pm

Alright thanks for the tips, looking forward to drop $250 on an argon tank..
User avatar
  • Posts:
  • Joined:
    Thu Dec 26, 2013 12:41 am
  • Location:
    Laredo, Tx

Gotta pay to play. Search your craigslist first. I've scores lots of empty tanks for $75-$100. Just have to make sure your LWS accepts trade-in's that you "own".
Image
varekai
  • Posts:
  • Joined:
    Fri Aug 02, 2019 6:03 pm
  • Location:
    Paso Robles, CA

Juliano_R wrote:Alright thanks for the tips, looking forward to drop $250 on an argon tank..
You might be able to take your C25 tank back, even if its not empty and exchange for pure argon, that way you just pay for the argon and not another tank. My lws says a tank is a tank, you don't have to get what you bring in. good luck!
User avatar
  • Posts:
  • Joined:
    Mon Feb 26, 2018 1:52 am
  • Location:
    Idaho

Don't buy a tank that is stamped with a company name at the neck (its not an owners) and make sure you can trade it like others said.
225256
  • Posts:
  • Joined:
    Thu Feb 23, 2017 12:35 am

Juliano_R wrote:
Juliano_R wrote:I got an eastwood tig 200, I have a 75% co2 argon mix @ 15 cfh and running with a 3/32 tungsten set at 110 amps. The steel is 3/16" and it wasn't cleaned before use. I know that it should be cleaned with a wire brush but I was too lazy to pull out the grinder :roll: . However I don't dip the tungsten in the weld pool and it still has trouble keeping a pointy tip.
forgot to mention, running 0.1s pre flow and 4seconds post flow
Some people say a rule of thumb for post flow is 1 sec for every 10 amps.
User avatar
  • Posts:
  • Joined:
    Wed Aug 21, 2019 5:43 pm
  • Location:
    Cape Cod, MA

Juliano_R wrote:Alright thanks for the tips, looking forward to drop $250 on an argon tank..
You can buy a 125 cf argon cylinder full of gas delivered to your door for free from Amazon. Have done this and was very happy. More than half the price of my LWS


Sent from my iPhone using Tapatalk
Learning is the best part of life and the most painful
Post Reply