Stick Welding Tips, Certification tests, machines, projects
What is that?TEACHDRM wrote:We know about the 6010/7018 and mineral oil one
One demonstration our instructor used was, he got a long bar of steel and welded two pieces of steel coming off the bar with "T" joints. One of the pieces he welded with 7018 and the other with hard surfacing rod. Then he broke them off with a hammer to show the difference between hardness and strength/ductility.
Farmwelding
- Farmwelding
-
Weldmonger
-
Posts:
-
Joined:Thu Mar 10, 2016 11:37 pm
-
Location:Wisconsin
I always enjoy scratching a 6010 on some plate and then polishing and bending it to see how devastating arc strikes can be. Or tacking a piece of angle iron to a table a foot in and then putting a tack on it and putting all my weight on it and then simply lift it up and break the tack to show how important weld placement is.
A student now but really want to weld everyday. Want to learn everything about everything. Want to become a knower of all and master of none.
Instagram: @farmwelding
Nick
Instagram: @farmwelding
Nick
Yes, If you take 3 identical plates and weld one 6010, the other 7018 rod left out of the oven (the longer the rod is left out the better results) and 7018 directly from the oven and place them in container of mineral oil you can see the hydrogen gas bubbles coming out of the welds. This shows why proper storage of rod is important. There is a youtube video that shows a really nice example.Lightning wrote:What is that?TEACHDRM wrote:We know about the 6010/7018 and mineral oil one
One demonstration our instructor used was, he got a long bar of steel and welded two pieces of steel coming off the bar with "T" joints. One of the pieces he welded with 7018 and the other with hard surfacing rod. Then he broke them off with a hammer to show the difference between hardness and strength/ductility.
https://youtu.be/H4aSkugbcaA
Huh. Never saw anything like that before. I'm surprised the hydrogen isn't "dissolved" in the weld deposit, and thus "trapped forever" in the steel. I don't understand how it's getting out to bubble through the oil. (Or maybe that's just the hydrogen trapped at the very edge, the very top surface layer, of the weld deposit? Or is the weld deposit "honeycombed" at a microscopic level with microscopic, interconnected porosity that lets the hydrogen escape?)TEACHDRM wrote: Yes, If you take 3 identical plates and weld one 6010, the other 7018 rod left out of the oven (the longer the rod is left out the better results) and 7018 directly from the oven and place them in container of mineral oil you can see the hydrogen gas bubbles coming out of the welds. This shows why proper storage of rod is important. There is a youtube video that shows a really nice example.
https://youtu.be/H4aSkugbcaA
- MinnesotaDave
-
Weldmonger
-
Posts:
-
Joined:Sun Oct 27, 2013 10:57 pm
-
Location:Big Lake/Monticello MN, U.S.A.
This paper could clear it up for you. I think it's pretty well written. http://www.jwri.osaka-u.ac.jp/publicati ... 421-07.pdfLightning wrote:Huh. Never saw anything like that before. I'm surprised the hydrogen isn't "dissolved" in the weld deposit, and thus "trapped forever" in the steel. I don't understand how it's getting out to bubble through the oil. (Or maybe that's just the hydrogen trapped at the very edge, the very top surface layer, of the weld deposit? Or is the weld deposit "honeycombed" at a microscopic level with microscopic, interconnected porosity that lets the hydrogen escape?)TEACHDRM wrote: Yes, If you take 3 identical plates and weld one 6010, the other 7018 rod left out of the oven (the longer the rod is left out the better results) and 7018 directly from the oven and place them in container of mineral oil you can see the hydrogen gas bubbles coming out of the welds. This shows why proper storage of rod is important. There is a youtube video that shows a really nice example.
https://youtu.be/H4aSkugbcaA
Dave J.
Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~
Syncro 350
Invertec v250-s
Thermal Arc 161 and 300
MM210
Dialarc
Tried being normal once, didn't take....I think it was a Tuesday.
Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~
Syncro 350
Invertec v250-s
Thermal Arc 161 and 300
MM210
Dialarc
Tried being normal once, didn't take....I think it was a Tuesday.
Artie F. Emm
- Artie F. Emm
-
Weldmonger
-
Posts:
-
Joined:Thu Jul 24, 2014 7:53 am
One of Jody's videos features a 7014 rod in a stinger, no human touch involved, balanced so the weld end of the electrode is held by gravity against the workpiece. The arc strikes and the electrode feeds itself into the weld.
Not really an "experiment" but possibly good for a demo, or a lesson in holding a tight arc.
Not really an "experiment" but possibly good for a demo, or a lesson in holding a tight arc.
Dave
aka "RTFM"
aka "RTFM"
Farmwelding
- Farmwelding
-
Weldmonger
-
Posts:
-
Joined:Thu Mar 10, 2016 11:37 pm
-
Location:Wisconsin
And showin how forgiving the 7014 isArtie F. Emm wrote:One of Jody's videos features a 7014 rod in a stinger, no human touch involved, balanced so the weld end of the electrode is held by gravity against the workpiece. The arc strikes and the electrode feeds itself into the weld.
Not really an "experiment" but possibly good for a demo, or a lesson in holding a tight arc.
A student now but really want to weld everyday. Want to learn everything about everything. Want to become a knower of all and master of none.
Instagram: @farmwelding
Nick
Instagram: @farmwelding
Nick
Thanks, MinnesotaDave. I'm somewhat familiar with the concept of hydrogen embrittlement, and why 7018 used for code work needs to be kept dry in an oven, but I never saw the demonstration with the hydrogen bubbling out of the steel. I just kind of scanned the article...does it explain how the hydrogen is (apparently) getting out of the weld deposit?MinnesotaDave wrote:This paper could clear it up for you. I think it's pretty well written. http://www.jwri.osaka-u.ac.jp/publicati ... 421-07.pdf
You want him to read it for you also?Lightning wrote:Thanks, MinnesotaDave. I'm somewhat familiar with the concept of hydrogen embrittlement, and why 7018 used for code work needs to be kept dry in an oven, but I never saw the demonstration with the hydrogen bubbling out of the steel. I just kind of scanned the article...does it explain how the hydrogen is (apparently) getting out of the weld deposit?MinnesotaDave wrote:This paper could clear it up for you. I think it's pretty well written. http://www.jwri.osaka-u.ac.jp/publicati ... 421-07.pdf
Return to “Stick Welding/Arc Welding - Shielded Metal Arc Welding”
Jump to
- Introductions & How to Use the Forum
- ↳ Welcome!
- ↳ Member Introductions
- ↳ How to Use the Forum
- ↳ Moderator Applications
- Welding Discussion
- ↳ Metal Cutting
- ↳ Tig Welding - Tig Welding Aluminum - Tig Welding Techniques - Aluminum Tig Welding
- ↳ Mig and Flux Core - gas metal arc welding & flux cored arc welding
- ↳ Stick Welding/Arc Welding - Shielded Metal Arc Welding
- ↳ Welding Forum General Shop Talk
- ↳ Welding Certification - Stick/Arc Welding, Tig Welding, Mig Welding Certification tests - Welding Tests of all kinds
- ↳ Welding Projects - Welding project Ideas - Welding project plans
- ↳ Product Reviews
- ↳ Fuel Gas Heating
- Welding Tips & Tricks
- ↳ Video Discussion
- ↳ Wish List
- Announcements & Feedback
- ↳ Forum News
- ↳ Suggestions, Feedback and Support
- Welding Marketplace
- ↳ Welding Jobs - Industrial Welding Jobs - Pipe Welding Jobs - Tig Welding Jobs
- ↳ Classifieds - Buy, Sell, Trade Used Welding Equipment
- Welding Resources
- ↳ Tradeshows, Seminars and Events
- ↳ The Welding Library
- ↳ Education Opportunities