Welding Certification test Q&A and tips and tricks
Post Reply
Jeffrey
  • Posts:
  • Joined:
    Sat Mar 26, 2011 10:49 am

I have been testing at a local paper mill on 2" 304 SS using solar flux for the backing. They have us using alcohol to mix it. It seems very common to get one or two small spots of sugar on the root (the CWI seems to not be concerned). Would using methanol instead of alcohol fix the problem?
User avatar
  • Posts:
  • Joined:
    Thu Jan 06, 2011 11:40 pm
  • Location:
    Near New Orleans

See my reply @ your duplicate post on the tig forum.

Steve
Post Reply