flux core technique.
Posted: Tue Oct 15, 2013 6:27 am
Hey Jody,
I have been talking about a flux core technique lately, that involves leaving the slag on the weld between runs. This is for multi pass multi layer fillet welds and supposedly aids bead formation, (removed each layer) The people who do it swear by it but to the uninitiated, it sounds like crap. Just wondering if you could give it a crack. Ps im talking 1/2" plus weld size.
Regards Mick.
I have been talking about a flux core technique lately, that involves leaving the slag on the weld between runs. This is for multi pass multi layer fillet welds and supposedly aids bead formation, (removed each layer) The people who do it swear by it but to the uninitiated, it sounds like crap. Just wondering if you could give it a crack. Ps im talking 1/2" plus weld size.
Regards Mick.