by Scott Young94
Wed Feb 20, 2013 12:22 am
Forum: Mig and Flux Core - gas metal arc welding & flux cored arc welding
Topic: stick out
Replies: 4
Views: 1451

Re: stick out

too long of a stick out will increase your splatter and cause your weld profile to be more convex. The reason is the longer the stick out the higher the resistance of the current flowing through the wire thus heating it up. This will affect your voltage and because you are running a CV unit, the mac...
by Scott Young94
Tue Feb 19, 2013 11:34 pm
Forum: Mig and Flux Core - gas metal arc welding & flux cored arc welding
Topic: ZTFab's welding method
Replies: 1
Views: 1371

ZTFab's welding method

Jody, I posted this over on Welding Web and thought I would copy and paste it here. Thank you for the hard work you put into making these videos. This is a video of Jody showing his torch movement when welding mig. It is the same as I was taught as well as many other's over the years. http://www.you...